Updated time: 2021-11-15 11:09:35
26A-1030605
TW I552420、PCT
This technique provides a cheap and low-cost process to integrate the manufacturing of battery material and coating process of battery electrode into one-step process. The thickness of the coated material is tunable to reach 10~100 micrometer (or even thinner) that is 1/2~2/3 thinner than the conventional cathode coated on the current collector for lithium ion battery. The specific capacity can achieve 1400mAh/g and its energy density is 2800Wh/Kg.
- One-step process for the manufacturing of battery material and coating of battery material with low cost
- The thickness of battery material can be tuned by the sprayed process; it is potential to fabricate the flexible thin battery with low cost.
- Energy density can achieve 2800 Wh/Kg
- The conducting agents, such as SuperP, KS6 etc. are not content during this spraying process.
- The whole process is operating at room temperature.
This technique provides a total solution to the battery material and cell companies that it can integrate the manufacturing of battery material and material coating into one-step process.
Chih Wei Chu、Lain-Jong Li、Pushpendra Kumar、Lung-Hao Hu
If you are interested in this technology, please fill in the information on the webpage under the manufacturer option (Request for Technology Licensing, Material Transfer, or Sponsored Research) on the website of this office

THE PREPARATION OF LITHIUM, SULFUR AND CARBON WITH CATHODE AND ANODE MATERIALS FOR LITHIUM ION BATTERTY AND THE METHOD THEREOF